Color:
Other
Compressive Strength:
63.56 Newtons per Millimetre Squared (N/mm2)
Weight:
40 Kilograms (kg)
SO3 %:
4%
Fineness:
Fine
Bending Strength:
33 Mpa
MgO %:
44.27 %
Initial Setting Time:
30 Minutes
Cement Raw Material:
Silicate
Cement Type:
Other
Sand Type:
Natural Sand
Sand Fineness:
Fine
Natural Sand Type:
Sand
Hardening Feature:
Rapid Hardening
Heat of Hydration:
Low Heat
Product Strength Grade:
River Sand
Feature:
Expansive, Volume stability, Other
This corrosion resistance silicates natural river sand. Sandblasting, glass beading and paint protection of equipment and surfaces. This SO3 4% and bending strength 33 MPA material is suitable for use as a cement additive, refractory bricks and ceramics, glass bead making, arc furnaces and brickworks. The MgO 44.27% silicate component of this natural river sand chemically bonds with your concrete, expanding and contracting with it to keep it intact over time. As the compressive strength of 63.56 result from erosion and water currents flowing through the earth.
Color: | Other |
Compressive Strength: | 63.56 Newtons per Millimetre Squared (N/mm2) |
Weight: | 40 Kilograms (kg) |
SO3 %: | 4% |
Fineness: | Fine |
Bending Strength: | 33 Mpa |
MgO %: | 44.27 % |
Initial Setting Time: | 30 Minutes |
Cement Raw Material: | Silicate |
Cement Type: | Other |
Sand Type: | Natural Sand |
Sand Fineness: | Fine |
Natural Sand Type: | Sand |
Hardening Feature: | Rapid Hardening |
Heat of Hydration: | Low Heat |
Product Strength Grade: | River Sand |
Feature: | Expansive, Volume stability, Other |