MgO %:
10 %
Bending Strength:
40.8 Mpa
Color:
Grey
Compressive Strength:
53 Megapascals (MPa )
SO3 %:
3.6 %
Initial Setting Time:
30 Minutes
Weight:
50 Kilograms (kg)
Cement Type:
Portland Pozzolana Cement
Sand Type:
Natural Sand
Sand Fineness:
Medium
Heat of Hydration:
Low Heat
Product Strength Grade:
53
Feature:
Acid-Proof
This 53-grade cement beats regular cement in terms of performance and tensile strength. It often provides superior workability, 53 megapascals of compressive strength, and stronger resilience to water, chemicals, and extremely high temperatures. It is grey in color, weighs 50 kg, and has a bending strength of 40.8 Mpa. These are frequently employed in building projects that call for natural sand with a 30-minute initial setting time, minimal strength requirements, and low durability.
| MgO %: | 10 % |
| Bending Strength: | 40.8 Mpa |
| Color: | Grey |
| Compressive Strength: | 53 Megapascals (MPa ) |
| SO3 %: | 3.6 % |
| Initial Setting Time: | 30 Minutes |
| Weight: | 50 Kilograms (kg) |
| Cement Type: | Portland Pozzolana Cement |
| Sand Type: | Natural Sand |
| Sand Fineness: | Medium |
| Heat of Hydration: | Low Heat |
| Product Strength Grade: | 53 |
| Feature: | Acid-Proof |