Weight:
50 Kilograms (kg)
MgO %:
2.0
Compressive Strength:
33-35 Mpa Megapascals (MPa )
Color:
Grey
SO3 %:
2.8
Initial Setting Time:
170 Minutes
Bending Strength:
33 Mpa
Cement Raw Material:
Silicate
Cement Type:
Silicate Cement
Sand Type:
Natural Sand
Sand Fineness:
Ultra-Fine
Natural Sand Type:
Fine
Hardening Feature:
Extra Rapid Hardening
Heat of Hydration:
Moderate Heat
Product Strength Grade:
53 Grade
Feature:
Other
This cement is a material used in building construction, composed of a mixture of various minerals, typically including limestone, clay, and silica, that can be hardened when mixed with water. The compressive strength of cement can vary depending on the type of cement being used. Generally, the compressive strength of cement should range between 33 and 35 m pa. This 53-grade cement is a type of ordinary portland cement (opc) that conforms to the standards set by the bureau of indian standards (bis).
Weight: | 50 Kilograms (kg) |
MgO %: | 2.0 |
Compressive Strength: | 33-35 Mpa Megapascals (MPa ) |
Color: | Grey |
SO3 %: | 2.8 |
Initial Setting Time: | 170 Minutes |
Bending Strength: | 33 Mpa |
Cement Raw Material: | Silicate |
Cement Type: | Silicate Cement |
Sand Type: | Natural Sand |
Sand Fineness: | Ultra-Fine |
Natural Sand Type: | Fine |
Hardening Feature: | Extra Rapid Hardening |
Heat of Hydration: | Moderate Heat |
Product Strength Grade: | 53 Grade |
Feature: | Other |