SO3 %:
5%
Initial Setting Time:
40 Minutes
MgO %:
2%
Weight:
40 Kilograms (kg)
Compressive Strength:
55 Megapascals (MPa )
Fineness:
225 m2/Kg
Color:
Grey
Bending Strength:
4.75 Mm
Cement Raw Material:
Other, Limestone,Clay
Cement Type:
Portland Pozzolana Cement
Sand Type:
Natural Sand
Sand Fineness:
Coarse
Hardening Feature:
Extra Rapid Hardening
Heat of Hydration:
Low Heat
Product Strength Grade:
High
This high-quality portland pozzolana cement with low heat-hydrating properties, suitable for composite material and construction, such as floors and walls. It has 55 megapascals compressive strength and 4.75 mm bending strength along with 225 m2/kg. It takes 40 minutes for the initial setting. It has SO3 % at 5% and MgO % at 2%. This has high compressive strength and is durable in oxidizing environments. It has excellent resistance to chloride corrosion, alkali corrosion, and moisture absorption.
| SO3 %: | 5% |
| Initial Setting Time: | 40 Minutes |
| MgO %: | 2% |
| Weight: | 40 Kilograms (kg) |
| Compressive Strength: | 55 Megapascals (MPa ) |
| Fineness: | 225 m2/Kg |
| Color: | Grey |
| Bending Strength: | 4.75 Mm |
| Cement Raw Material: | Other, Limestone,Clay |
| Cement Type: | Portland Pozzolana Cement |
| Sand Type: | Natural Sand |
| Sand Fineness: | Coarse |
| Hardening Feature: | Extra Rapid Hardening |
| Heat of Hydration: | Low Heat |
| Product Strength Grade: | High |