43 Grade Acid Proof Low Heat Natural Sand Iron Aluminate Common Cement

Color:

Grey

Weight:

40 Kilograms (kg)

Bending Strength:

4.75 Mm

MgO %:

2%

Initial Setting Time:

30 Minutes

SO3 %:

2.8%

Compressive Strength:

35 Megapascals (MPa )

Cement Raw Material:

Iron Aluminate

Cement Type:

Common Cement

Sand Type:

Natural Sand

Sand Fineness:

Medium

Hardening Feature:

Rapid Hardening

Heat of Hydration:

Low Heat

Product Strength Grade:

43

Feature:

Acid-Proof

2026nd Year

Contact Person

14, Near TNCSC Godown,

Product Description

This product is a natural sand common cement that is made from iron aluminate material. This product has a medium sand fineness and rapid hardening. It has 43 strength grade and is acid-proof in nature. It contains 2.8% of SO3% and 2.0% of Mg0% and has 30 minutes of initial settling time. The compressive strength of this product is 35 megapascals and the bending strength is 4.75 Mm. This product is available in grey color and comes with a weight of 40 kilograms with low heat of hydration.

Color: Grey
Weight: 40 Kilograms (kg)
Bending Strength: 4.75 Mm
MgO %: 2%
Initial Setting Time: 30 Minutes
SO3 %: 2.8%
Compressive Strength: 35 Megapascals (MPa )
Cement Raw Material: Iron Aluminate
Cement Type: Common Cement
Sand Type: Natural Sand
Sand Fineness: Medium
Hardening Feature: Rapid Hardening
Heat of Hydration: Low Heat
Product Strength Grade: 43
Feature: Acid-Proof